TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Robert Peterson <[log in to unmask]>
Date:
Thu, 7 Oct 1999 15:53:18 -0400
MIME-Version:
1.0
X-To:
Jack Olson <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Robert Peterson <[log in to unmask]>
Parts/Attachments:
text/plain (62 lines)
Hi,

There is such a thing as soft electroless gold on printed circuits. It is
not applied instead of the immersion gold though. It needs an initial
immersion gold deposit because the chemistry is only catalytic on gold. Our
gold vendor sells the chemistry. Let me know if you are interested. It would
be used for wire bond with fine gold wire, not for soldering.

Bob

Robert Peterson
mailto:[log in to unmask]

Alternate Final Finishes, Inc.
166 Middlesex St.
N. Chelmsford MA 01863
Phone (978) 251-7429     Fax (978) 251-7219
http://www.AlternateFinalFinishes.com


-----Original Message-----
From: Jack Olson [mailto:[log in to unmask]]
Sent: Thursday, October 07, 1999 11:34 AM
To: [log in to unmask]
Subject: [TN] Flash Gold vs. ???


Do some manufacturers use the soft electroless gold (deep bath?) in place of
immersion gold? Is there some place I could learn what the difference is?
None of my books address it, and I always thought flash gold was a
self-limiting process that wouldn't go over 10 mils, but now we are hearing
it can be any thickness we want. True?

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2