TECHNET Archives

November 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Macko, Joe @ IEC" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Macko, Joe @ IEC
Date:
Tue, 30 Nov 2004 13:29:27 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (30 lines)
Fellow Technets,

Two smt type components we want to install on a gold plated pwb have from
0.5 to 1.0  um gold plating over 2 - 6 um of nickel.  J-STD-001C, paragraph
5.4.1, Gold Removal states that "Gold shall be removed from 95% of all
surfaces of surface mount components to be soldered regardless of gold
thickness".   The board is being assembled to class 3 requirements.  These
smt components are leadless type components with castellated terminations
provided on tape and reel and would not be easy to tin with solder .....

Would someone please help clarify this requirement.
Also, what is the latest IPC document that calls out the level of gold
required before "embitterment" is a concern.  Over the years, I have heard
and read numbers like 0.3 to 3% by wt. and from 5 to 100 u-inches. (Not sure
how to covert a (% by wt) value to a thickness?)

Looking forward to some comments. thanks

joe

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2