TECHNET Archives

June 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
James Mahoney <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, James Mahoney <[log in to unmask]>
Date:
Tue, 24 Jun 2008 09:15:30 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (166 lines)
Based on past real time experience 2 hours min @ 250 worked for any type of
soldering being performed including HAL and the operation being done within
4 hours. I have baked rigid flex up to .25 thick at at 4-6 hrs but only
during the summer months.

Moisture being absorbed into the board is minimal but very important to
remove prior to any extreme heat. Kapton and acrylic adhesive is the
concern.

Thank you,
Jim Mahoney
Quick Turn Flex Circuits, LLC
Applications Project Manager
P# 603-821-6571
F# 603-821-5723
M# 603-305-6250


** This email and all attachments have been scanned prior to being sent**
Confidentiality Notice: This page and any accompanying documents contain
information that is confidential, privileged or exempt from disclosure and
is intended for the exclusive use of the addressee. If you are not the
intended recipient, you are hereby notified that any disclosure, copying,
distribution or use of the contents of this information in any manner is
strictly prohibited.



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Monday, June 23, 2008 3:21 PM
To: [log in to unmask]
Subject: Re: [TN] edge delamination flexible circuits assemblies

A bake of 250 F (126 C) for two hours could very well be just the right
bake time for a flex circuit.
The bake schedules listed in Handbook and J-STD-033 are guidelines, and
it is best if you determine the optimum bake schedule for any given flex
or PWB. I have detailed how this is done within this forum, check the
archives. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Kelly
Sent: Monday, June 23, 2008 1:16 PM
To: [log in to unmask]
Subject: Re: [TN] edge delamination flexible circuits assemblies

A 2 hour bake is not what IPC recommends for rigid flex. HDBK-001 says a
minimum of 6. Regards Steve Kelly

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of James Mahoney
Sent: June-23-08 1:06 PM
To: [log in to unmask]
Subject: Re: [TN] edge delamination flexible circuits assemblies

Without understanding the actual material being used it's difficult to
tell.
I would recommend cleaning with alcohol and bake prior to any assembly @
250 degrees for 2 hours and try and solder within 4 hours.

Thank you,
Jim Mahoney
Quick Turn Flex Circuits, LLC
Applications Project Manager
P# 603-821-6571
F# 603-821-5723
M# 603-305-6250


** This email and all attachments have been scanned prior to being
sent** Confidentiality Notice: This page and any accompanying documents
contain information that is confidential, privileged or exempt from
disclosure and is intended for the exclusive use of the addressee. If
you are not the intended recipient, you are hereby notified that any
disclosure, copying, distribution or use of the contents of this
information in any manner is strictly prohibited.




-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gabriela
Sent: Monday, June 23, 2008 1:11 PM
To: [log in to unmask]
Subject: [TN] edge delamination flexible circuits assemblies

What may cause the edge delamination of rigid/flex assemblies along the
edges of the flex connector?
We saw this defect only after cleaning the circuits in ABZOL .

Before assembly we are drying the circuits for several hours at 120C. Is
it possible that the cleaning process attacks the adhesive?

Are there recommendations for cleaning flexs?

Gaby


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2