TECHNET Archives

March 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset=us-ascii
Sender:
Subject:
From:
Reuven ROKAH <[log in to unmask]>
Date:
Wed, 31 Mar 2004 10:59:14 +0200
MIME-Version:
1.0
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (97 lines)
So am I,

0.2 mm + diagonal

0.3 mm + finished ID


Best  Regards

ROKAH Reuven




                      Brian Ellis
                      <b_ellis@PROTONI         To:      [log in to unmask]
                      QUE.COM>                 cc:
                      Sent by: TechNet         Subject: Re: [TN] Finished Hole Size vs Lead diameter
                      <[log in to unmask]
                      >


                      29/03/2004 17:34
                      Please respond
                      to "TechNet
                      E-Mail Forum.";
                      Please respond
                      to Brian Ellis





I don't know about a document, but I always used a rule of thumb, of 0.2
to 0.3 mm ID, after plating, greater than the diagonal or diameter of
the lead. FWIW.

Brian

Victor G. Hernandez wrote:

> Fellow TechNetters,
>
>     Can someone guide me to an IPC document that make reference to
> Finish Hole Size
> versus lead acceptable lead diameter with respect to ROUND, RECTANGULAR
> and SQUARE
> Leads.   I have a case in which the square lead deformed the PTH and
> minimal solder
> fillet is exhibited inside the barrel.   At least in my opinion.
>
> In advance I thank you for your timely response in this matter.
>
> Victor,
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2