TECHNET Archives

March 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Brian Ellis <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Date:
Tue, 22 Mar 2011 18:47:08 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (71 lines)
Very difficult! As I see it, why is there corrosion there, in the first 
place? A good acrylic coating should protect the boards, even better 
than most other coating types. As it apparently doesn't, this implies 
that moisture is being "pumped" in through the coating, in turn implying 
you have bad ionic/hygroscopic contamination between the board and the 
coating. What are your flux type, cleaning process and process control 
method before applying the coating?

Your first step towards recovery, if it is possible (not certain) is a 
good removal of all traces of acrylics. Consult your supplier to find 
out the best solvent for this and hope it does not damage any of the 
components. You must then remove all traces of the corrosion and any 
other residual contamination. My best guess, for a first try, would be 
methanol (warning! TOXIC/FLAMMABLE),preferably with strong agitation.

Brian

On 22/03/2011 17:00, Hetal Shah wrote:
> Hello,
>
>
> We have been using the acrylic  coating and it is failing.  My application
> is a small, expensive  copper/solder circuit board which must operate
> exposed in a greenhouse environment with humidity up to at least 80 per cent
> and temperature from about 55 to 85 deg F.  There is evidence of green
> corrosion products and peeling conformal coating which presumably need a
> more appropriate coating.
>
> We have to do rework and use agin same pcb boards. We would be very grateful If
> anyone can be advised how to remove corrosion from the board.
>
>
>
> thanks
>
> Hetal Shah
>
> MG Chemicals
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2