Hi, Howard,
PC501 is two- type epoxy curable solder mask commonly used during the past
and gradually replaced by photoimagble solder mask. It is understandable
someone know nothing about this solder mask. For the simple or better
performance, I suggest you talk to your customer to change it to the modern
types.
At 02:15 PM 1999/4/9 +0800, Howard Lin wrote:
>Dear TechNeters,
> Our customer ask us to use PC501 solder mask, but I do not know what it
>is. Can somebody tell me what it is and where I can get some information
>on this material?Any input I shall be very appreciated.
>
>Howard
>Maxedge Electronic Corp.
>[log in to unmask]
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|