TECHNET Archives

February 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 29 Feb 2012 18:14:38 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Message-ID:
Subject:
From:
Joyce Koo <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (52 lines)
If it is on wipe zone, you might have porous gold plating or thin gold plating layers.  Or some one used soft gold instead (used left over soft gold platingbath for connector as a cheap way.  Instead of real hardening gold with Ni, Co. 
--------------------------
Sent using BlackBerry


----- Original Message -----
From: Brian Ellis [mailto:[log in to unmask]]
Sent: Wednesday, February 29, 2012 01:01 PM
To: [log in to unmask] <[log in to unmask]>
Subject: Re: [TN] Field Return Product w/corrosion product

All fluxes, by definition, must have some form of corrosive ion for it 
to be able to reduce metal oxides. Even pure rosin isomers have a 
carboxylic acid group. From your description, it seems probable that you 
have what is effectively a short-circuited battery with gold and copper 
as your electrodes with bare copper where the fingers are cut or the 
gold plating is too thin/porous/worn through. Any condensation would 
provide you with an electrolyte, exacerbated by tthe presence of any 
ionogenic and/or hygroscopic contaminant (not necessarily from your 
flux, which you don't want on gold-plated fingers, anyway).

Brian

On 29/02/2012 16:53, Victor Hernandez wrote:
> Fellow TechNetters;
>
>     Do No Clean LF fluxes, Rosin Core/molten solder, have a corrosive ion?   Every so often when conducting analysis on Field Return Product I notice small amount of corrosion product on gold plated contact on DIMM and PCI Slot connector.   Sometimes on other gold plated connector leads.   So I am trying to understand which component had a corrosive ion waiting for the right conditions to flourish.   Small amount of greenish/bluish residue.   It can be seen on wipe zone and/or stamp edge of contact.   Where is this active corrosive ion coming from?
>
>     Can someone provide the link to Stevezea home page for posting pictures?
>
> Victor,
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2