TECHNET Archives

March 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 4 Mar 2009 11:06:05 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Kevin Glidden <[log in to unmask]>
Subject:
From:
Kevin Glidden <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (52 lines)
Thanks everyone, especially Doug!  Great info...
 


Kevin Glidden


-----Original Message-----
From: Kevin Glidden [mailto:[log in to unmask]] 
Sent: Wednesday, March 04, 2009 8:27 AM
To: [log in to unmask]
Subject: [TN] Gloved Hands / Fingerprints / Failure Articles

Hello everyone,
 
We are in the midst of a proposal from myself and manufacturing engineering
to require use of gloves or finger cots throughout our PCB assembly process.
We had considered that it really would only be required after final
cleaning, but for uniformity would require it all steps including
population.  We have of course met with a real resistance, particularly from
the final assemblers who are stating it doesn't matter once the conformal
coat is on.  I can see at least some logic in that, and admittedly a large
portion of our argument is aesthetics (we don't want fingerprints on the
boards even after coating), but it would be really nice to have some sort of
scare tactic, like an article or something that related a PCB failure to
fingerprints or handling contamination.  Anyone have such a thing?
 
Thanks!

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2