TECHNET Archives

March 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Eltek Ltd. - Process Engineering" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 26 Mar 1998 09:24:24 +0300
Content-Type:
text/plain
Parts/Attachments:
text/plain (41 lines)
At 11:03 25/03/98 -0500, you wrote:
>In my experience the following adv./disadv. apply to carbon and gold
>contacts.
>

>Gold
>Advantage               - Less process steps ( lower cost? ) if flash plate
all over.
>                        - Smaller footprint for tight designs.

>Keith Lumley
>RexCan Circuits Inc.


Hi !
This statement is grate mistake !!!
 " Flash it over " it means , plating Nickel-Gold on unteched copper  while
Nickel-Gold is used further etch resist for copper . This is time consuming
operation , problematic yields , poor resolution , very problematic  for
fine lines and dense SMD . There are some ways to plate on etched boards ,
but this the board must be re-design .


Edward Szpruch
Eltek Ltd - Israel
Tel  972 3 9395050
Fax 972 3 9309581
E-mail :  [log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2