TECHNET Archives

November 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Werner Engelmaier /* <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 7 Nov 2007 08:02:25 EST
Content-Type:
text/plain
Parts/Attachments:
text/plain (53 lines)
Hi Badri,
Your 'Subject' line says: "Delamination of lead free PCBs," but your problem 
has nothing to do with delamination.
You have in fact 2 problems not related to any delamination.
(1) the thickness of the inner-layer traces is not thick enough according to 
specifications and your customer belives that the current carrying [not 
voltage] capacity of the 35 micron tracks is insufficient for their use. Whether or 
not this is in fact true is immaterial—the PCBs have not been manufactured to 
spec.
No salvage for these PCBs.
(2) there are discontinuities in the PCB interconnects on over 50% of the PCBs
—you do not give any details on the responsible failure mode. This could be 
either because of via barrel cracking or inner-layer (post) separation—no way 
of knowing without x-sections.
No salvage for these PCBs.

ACTION ITEMS:
(1) Do a failure mode analysis—this will tell you what needs fixing.
(2) From (1) you can tell whether the design is adequate for Pb-free 
soldering or whether the root cause is production quality [track thickness and/or 
other reasons]. 
If it is a design/specification issue, you may want to get my White Paper 
"Recommendations for PCB FAB Notes and Specifications in Printed Circuit Board 
Drawings for SnPb and Lead-Free Soldering Assemblies, the Qualification of PCB 
Shops and Activities to Assure Continued Quality."
If it is a quality issue, fix it.



Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com



**************************************
 See what's new at http://www.aol.com

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2