TECHNET Archives

April 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Mike Bailey <[log in to unmask]>
Date:
Thu, 22 Apr 1999 09:01:34 -0700
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Mike Bailey <[log in to unmask]>
Parts/Attachments:
text/plain (30 lines)
Got an age old problem.  Maybe there are some new solutions.  We're building
some conventional sub-assy blind via boards that have via in pad
configurations.  No big surprise, the electroless copper adhesion on the
resin-fill areas is blistering.  Re-design using laser drilling is not an
option, nor is direct plate technology or plasma.  We have tried the usual
pre-electroless copper bake as well as post-bake, mechanical scrubbing etc.
etc.  I'm a little hesitant to play with additional desmear tactics as they
have a tendency to or smooth out the original surface texture.

Also as usual, I don't have much time.

Material is conventional 140 Tg epoxy
Hole dia. is .0118.
Yes, some surface sanding is required after final lamination (just like the
rest of you guys)!!

Any ideas?

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2