TECHNET Archives

February 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Genny Gibbard <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Genny Gibbard <[log in to unmask]>
Date:
Fri, 9 Feb 2007 09:50:01 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (59 lines)
First of all, to cut our stockroom people some slack - this is the
general stockroom, not the SMT stores where things might be stored
partially consumed.  Anything stored in this fridge is still sealed and
new stock from receiving that hasn't been issued out yet.  I think some
of the guys there almost never leave that area.  The lunchroom and only
other fridge option is on the complete opposite end of the building.

The containers are all still sealed, unopened.  I guess I should have
been more specific - my question is how/where do you recycle it?  I am
having trouble finding any place convenient to the center of the
Canadian prairies.  We also don't have a wave solder pot in house.
Maybe I'll contact the wave solder contractor we use ...

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Sauer, Steve
(Xetron)
Sent: February 9, 2007 9:33 AM
To: [log in to unmask]
Subject: Re: [TN] What to do with expired solder paste?

Hi Genny,
First off, from a safety perspecitve, a dedicated refrigerator should be
used to store solder pastes and other chemicals away from human
consumables.
In the past, I have dumped expired solder paste in the wave solder pot
and tinning solder pots.  One other option is to dispose of it as
hazardous waste.

Good luck!

Steve
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard
Sent: Friday, February 09, 2007 10:26 AM
To: [log in to unmask]
Subject: [TN] What to do with expired solder paste?

Was sorting through the fridge in the stockroom at work...pushed aside a
couple of sandwiches and yogurts (the stockroom people keep their
lunches in there...) and came across a box with 9kg(18 jars) of solder
paste expired in mid 2004 - a brand we don't use any more.  Standard
63/37 no-clean.

What would you do with it?  Never even been opened.

Genny.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2