Sounds like you might be witnessing moisture in the solder mask itself.
Solder mask, even fully cured, is porous and under certain circumstances can
exit your equipment (including drying) with a white hazy appearance across
the mask covered areas.
One method to test this is to bake a unit around 150F for a couple hours and
see if this goes away.
Franklin
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Charlie Pitarys
Sent: Tuesday, December 11, 2007 2:19 PM
To: [log in to unmask]
Subject: [TN] Ghost white marks on LPI solder mask
I know this has been brought up several times. Searched the archives but
more help will be appreciated.
Full process:
Before Reflow PCB have Temperature storage at 65°C for a minimun of 24H
(some time few weeks)
After Refow before wave solder the PCB have Temperature storage at 70°C
for 8 hours (the night)
After Wave solder (Pacific 9000M flux) 100% of production is cleaned.
Current
wash temp. was set at 70C. Yes I know this is extreme and advised to
lower<60C. This helped a little.
If a sample section PCB is protected with Kapton and Kapton removed before
cleaning No Problem appears on that solder mask area.
You can even see an outline where the wave solder fingers caused shadowing
of the solder mask and on the top side along the edge where some flux has
wicked over.
I need to direct my customer to documents, etc. that have substance on this
issue. He is hesitant to receive my advise and reasons that I know for this
occurance. Bad solder mask.
The problem of white mark is only on few case (less than 5% of PCB).
The PCB I saw was subjected, before any process a Temperature storage of
65°C during 3 weeks (can this make the PCB more sensitive ?)
My flux analysis shows the spectrum has all the signature features for a
carboxylic acid and a library search brought up adipic acid as the closest
match.
Thanks in advance
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|