Gary,

Most laminate Suppliers will give you a nominal Er based on a 50/50
glass to resin ratio...if you talk to them they may even have a curve
of Er based on the ratio of glass to resin in a package..the true Er is
based on this ratio...Typically for FR4 it runs between 4.1 and 4.6 as
the ratio changes...for general calcualtions I use a 4.3 Er at 50%
glass and 50% resin..when you look at your package you should try to
estimate if you will be above or below this range..then you can
estimate the effect...the best way to know is to have a particular
construction tested...

Doug Jeffery
Engineering Mangaer
Electrotek, Inc.

Email: [log in to unmask]

You wrote:
>
>Does anyone know where I can find information on the dielectric
constants of pre-preg materials used for PCBs?
>
>
>Gary
>
>
>
>==================================================
>
><color><param>0000,0000,ffff</param>Gary Griffin
>
>Engineering Manager
>
>Phone (408) 501-7156
>
>Fax   (408) 437-1976
>
>Pager 1-800-759-7243 Pin: 145-1886
>
>Alpha pager email griffin_p or [log in to unmask]
>
>SABER group Interface Products</color>
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
additional information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>################################################################
>
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2