TECHNET Archives

March 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Date:
Tue, 11 Mar 2003 10:21:27 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Charles Caswell <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Charles Caswell <[log in to unmask]>
Parts/Attachments:
text/plain (186 lines)
I just brushed or dipped the parts followed by 2 rinses with R.O water. For disposel we neutralized the SolderNu with baking sod
Charles Caswell 

-----Original Message-----
From: Black, Paul [mailto:[log in to unmask]]
Sent: Tuesday, March 11, 2003 9:55 AM
To: [log in to unmask]
Subject: Re: [TN] Kester Solder-Nu replacement


Dear Technetters,

We recently found some socketed PLLC's that were returned from customers
with lead contamination. The parts are otherwise fine. Would Solder-Nu be a
good candidate to remove this contamination? How is it applied? What
methods) are normally used for disposal when the chemical is spent?

Thank you,
Paul Black
Manufacturing Engineer
Kronos


-----Original Message-----
From: Charles Caswell [mailto:[log in to unmask]]
Sent: Wednesday, March 05, 2003 10:10 AM
To: [log in to unmask]
Subject: Re: [TN] Kester Solder-Nu replacement


I just received this. I just want to keep things accurate on the forum.



Dear Mr. Caswell,

The Kester # 5560, Solder-Nu has not been discontinued.  I am attaching the
Data Sheet for this product.

This product is available through distribution.  To find a distributor near
you go to the Kester home page and click on the Distributors button and
scroll down to your state to locate a distributor near you.

We appreciate your interest in Kester products and if there is anything
additional we can do for you feel free to contact us further.

Thanks,

Dave Scheiner
[log in to unmask]

-----Original Message-----
From: Dave Hillman [mailto:[log in to unmask]]
Sent: Friday, February 28, 2003 11:01 AM
To: [log in to unmask]
Subject: Re: [TN] Kester Solder-Nu replacement


Hi Charles! The SolderNu product was fluoboric acid based instead of
phosphoric acid based. Kester is discontinuing the SolderNu product?
Bummer, when used carefully the stuff was a nice tool to have in the
solderability restoration kit!

Dave



                      Charles Caswell
                      <CharlesC@FESCORP        To:       [log in to unmask]
                      .COM>                    cc:
                      Sent by: TechNet         Subject:  Re: [TN] Kester
Solder-Nu replacement
                      <[log in to unmask]>


                      02/26/2003 04:00
                      PM
                      Please respond to
                      "TechNet E-Mail
                      Forum."; Please
                      respond to
                      Charles Caswell






Sorry I don't have the msds anymore. I just remember it was phosphoric acid
based. Smelled just like the descaler I use in my aqueous machine. So when
I read that it was discontinued I dug into some parts we use for training
and found some resistors that are pretty ugly. Soaked in descaler for about
a minute, rinsed and tinned. It worked. If your quality dept. is like ours
though it would be a hard sell.
Charles Caswell

-----Original Message-----
From: Phil Nutting [mailto:[log in to unmask]]
Sent: Wednesday, February 26, 2003 12:56 PM
To: [log in to unmask]
Subject: [TN] Kester Solder-Nu replacement


I've just been informed that Kester has discontinued Solder-Nu.  Does
anybody know of a similar product by any other manufacturer?

Phil Nutting

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
 -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2