TECHNET Archives

December 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
KELLY M SCHRIVER <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 16 Dec 1998 15:20:00 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (40 lines)
Hi Ralph -

Just a few quick comments:

In general, ever since the origins of "popcorning" were determined, both the
assembly and components industry have taken the approach to keep the parts dry
and dehumidified.  There have been many published reports on the phenomena.

There are a number of grades of plastics, which have varying periods of
"floor life" during which they can safely withstand reflow temperatures.
"Floor life" being that period before the plastic has absorbed sufficient
moisture to be at risk.

The objective is to avoid "popcorning" not let it crack and then keep stuff
out of the cracks.  Their logic for this decision would seem very questionable.

Have your folks considered the issues of attempting to conformal coat over no
clean residues?  (Particularly with some of the low VOC coatings, which don't
tend to take some of the lower grade process residues into solution.)

By the way, the Motorola folks have quite a number of pubs available on the
care and feeding of their parts relative to this subject.

Well, that's all for the moment.  I'm sure the others will have a great deal
to add.

Good luck - Kelly

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2