TECHNET Archives

October 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Date:
Tue, 29 Oct 2002 19:37:00 -0600
Content-Disposition:
inline
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Content-type:
multipart/mixed; Boundary="0__=XbFmsrN92UsyBnlRF74iHbfWk4ATyoRt10P0nwoVnsEKjJ2vLgNzccyB"
Subject:
From:
"Jason W. Gregory" <[log in to unmask]>
Parts/Attachments:
text/plain (2100 bytes) , att1.htm (1201 bytes)


I will second Steve's comment on 2% silver paste. Right on, bro!

Jason Gregory




Steve Gregory <[log in to unmask]> on 10/29/2002 06:37:18 PM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to
      [log in to unmask]

To:   [log in to unmask]
cc:    (bcc: Jason Gregory/LABARGE)

Subject:  Re: [TN] Round Pads for 0402 Parts?



Hi Rick!

I'll get back to you tomorrow with some pad geometries that have worked well
here...don't trust my memory (getting senile, ya' know...hehehe)

Have you tried using a 2% silver solder paste yet? I'd recommend it very
highly!!
Believe me, it makes a HUGE difference!!!!

-Steve Gregory-

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------


ATOM RSS1 RSS2