TECHNET Archives

July 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Werner Engelmaier <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 19 Jul 2005 11:33:21 EDT
Content-Type:
text/plain
Parts/Attachments:
text/plain (24 lines)
Hi Vladimir,
You are correct.
I have never seen an overstress failure of a solder joint that involved voids
in the solder joint bulk volume. I have seen creep-fatigue failures in SJs
with voids that did not involve the voids at all, or that went through the
voids, but were not caused by them. I have even seen SJs with cracks in them where
the cracks stopped at a void.
Overstress failures invariably involve the interfaces of solder joints where
for a variety of reasons really weak 'links' were created; that includes
interfacial failures due to Kirkendall voids.

Regards,
Werner Engelmaier

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2