If specimens acn be put into a SEM/EDX system, you can at least get an
elemental suggestion of what it is...
> -----Original Message-----
> From: [log in to unmask] [SMTP:[log in to unmask]]
> Sent: Wednesday, August 12, 1998 2:39 PM
> To: [log in to unmask]
> Subject: [TN] Unidentified Material Between Conductors
>
> All,
>
> We are having some problems with a backplane PCB. There appears to be
> some sort
> of material bridging some conductors under the conformal coat on the
> solder side
> of the PCB.
>
> The material appears in various colors, but mostly appear as a
> blue-green to
> black color. This material is also conductive (which is how we found
> the
> problem.....the unit failed electrical test).
>
> The boards are not subjected to any environmental stresses prior to
> discovering
> this problem.
>
> Any hints or suggestions?? E-Mail me for additional information
> (Photo's will
> also be available soon).
>
>
> Steve
> [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|