Mime-Version: |
1.0 |
Content-Type: |
text/plain; charset=ISO-8859-1; name="ASSY:Oil" |
From [log in to unmask] Fri Aug 16 16: |
15:14 1996 |
Old-Return-Path: |
|
Date: |
Fri, 16 Aug 96 13:12:32 +0200 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
Content-Transfer-Encoding: |
7bit |
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Status: |
|
Resent-Message-ID: |
<"FXXH91.0.ue5.aR55o"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
X-Openmail-Hops: |
1 |
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0urMmM-0000KoC; Fri, 16 Aug 96 06:09 CDT |
Message-Id: |
<H00004850061c68d@MHS> |
Parts/Attachments: |
|
|
Technetters,
I'm just curious about the affect on component solderability after used
a bend&cut machine. I suspect some kind of lubricant coating after using
these machines on our components. The machines need this to operate
properly.
Is there any other kind of lubricant or some other solution to this?
How does oil affect the solderability?
Is there any low-cost way to remove this oil before wave soldering
without much time loss?
I'm greatful for anykind of info.
/Jan Merstrand
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|