Hi Lou:
Graham Collins provided some great advice. I can think of only one more
thing to add and that is the size of the pot. We have a large pot, 1500 lb
+, Dover Soltec. Our run rates and the amount of solder added to keep the
pot at a certain level pretty much keeps the contamination level below the
limits. We still do solder analysis but not as often as with the older
Hollis machine which was a 650 lb pot. Graham is right about one thing to
watch carefully and that is if you expose the pot to a lot of gold, you may
want to check a little more often than twice a year. If you have a smaller
pot, you may want to reconsider the twice a year scenario. Your SPC data
will tell you how long you can go before changing the pot.
Our old Hollis with a 650 pound pot required us, at our run rates, to change
the pot every 6 weeks. The new Soltec with a pot, that I actually think is
1750 lbs, with auto solder feed, was more efficient and less costly to
maintain. The only time we emptied the pot was to work a pump issue which
has been very few times. As a matter of fact I think we only dumped the
solder once and that was for a pump or baffle upgrade. Anyhow hope this
helps a little.
Ron Hollandsworth
ITT
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|