If it really is debris, people have approached it over the years with high
pressure rinse modules after drill and when we had a shop we used a vapor
hone followed by a high pressure rinse module to clean the hole. Be aware
our experience was that vapor hones tend to eat themselves up and require
continuous maintenance. If it is a ring void them you have a different
problem and that is probably drilling parameter related or material degree
of cure. Are you peck drilling?
> -----Original Message-----
> From: Vickie Dycewicz [SMTP:[log in to unmask]]
> Sent: Tuesday, February 02, 1999 10:03 AM
> To: [log in to unmask]
> Subject: [TN] Removing Debris from Holes before Electroless
> Deposition
>
> I am looking for information on what companies are using to remove debris
> in
> holes before the electroless deposition (dep) process.
>
> We are getting pth voids in holes due to drill debris still in the holes
> after
> deburr, before dep. Cross section pictures of the pth void show a
> circumfrential
> void, near the center of the hole. The electroless copper leading up to
> the void
> is very granular, as if trying to dep over debris. I do not classify them
> as
> bubble voids because of the debris still left in the hole.
> I predominately see these voids in 0.022 holes, 0.261 panel thickness.
> After drill the panels are hand sanded, then through our deburr process
> which is
> an IS Scrubbex with 350psi high pressure spray section.
>
> I would greatly appreciate any suggestions on how to improve my process.
>
> Thanks,
> Vickie Dycewicz
> Electroless Deposition Process Engineer
> Teradyne, Inc.
> Nashua, NH
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|