TECHNET Archives

April 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Douglas Pauls <[log in to unmask]>
Date:
Tue, 14 Apr 2015 10:25:40 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Message-ID:
Subject:
From:
Steve Gregory <[log in to unmask]>
X-cc:
TechNet E-Mail Forum <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (78 lines)
Thanks Doug! So is there anything you can do, like wash them in alcohol or
something?

Steve

On Tue, Apr 14, 2015 at 10:23 AM, Douglas Pauls <
[log in to unmask]> wrote:

> Steve,
> In my experience they do.  We sometimes see the same thing, whether molded
> rubber or molded vinyl.
>
>
> Doug Pauls
> Principal Materials and Process Engineer
> Rockwell Collins
>
> On Tue, Apr 14, 2015 at 11:21 AM, Steve Gregory <[log in to unmask]>
> wrote:
>
>> Hi All,
>>
>> Just got some black ESD rubber masking boots for some blade terminals for
>> a
>> board that we dip in Humiseal 1A33, and noticed that there is shadowing
>> around the base of the terminals like something was repelling the coating
>> away from them, maybe some sort of mold release compound? Tried dipping
>> without the boots and we don't see the shadow. I got the boots to keep the
>> coating from getting on the terminals so that we weren't sitting there
>> with
>> a conformal coat removal pen cleaning the terminals up after we dipped the
>> boards.
>>
>> I called the manufacturer of the boots and asked about the issue, and he
>> said they would get back to me. Haven't heard anything yet. I'll try to
>> get
>> a picture that shows you what I'm talking about...
>>
>> Steve
>>
>> --
>>
>>
>> This email and any attachments are only for use by the intended
>> recipient(s) and may contain legally privileged, confidential, proprietary
>> or otherwise private information. Any unauthorized use, reproduction,
>> dissemination, distribution or other disclosure of the contents of this
>> e-mail or its attachments is strictly prohibited. If you have received
>> this
>> email in error, please notify the sender immediately and delete the
>> original.
>>
>>
>> ______________________________________________________________________
>> This email has been scanned by the Symantec Email Security.cloud service.
>> For more information please contact helpdesk at x2960 or [log in to unmask]
>> ______________________________________________________________________
>>
>
>

-- 


This email and any attachments are only for use by the intended 
recipient(s) and may contain legally privileged, confidential, proprietary 
or otherwise private information. Any unauthorized use, reproduction, 
dissemination, distribution or other disclosure of the contents of this 
e-mail or its attachments is strictly prohibited. If you have received this 
email in error, please notify the sender immediately and delete the 
original. 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2