Werner, Eddie,
The finished hole diameter is important only in one instance - when it is used for accurately-matched TH component, such as press-fit component. It is not relevant in case of connecting via (provided it is well-designed for curent carrying and signal integrity aspects).
Ofer Cohen
Seabridge
A Siemens Company
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
> Sent: Friday, May 13, 2005 01:48
> To: [log in to unmask]
> Subject: Re: [TN] board fab
>
> Hi Deac,
> Why is anybody still quoting finished hole diameters; for
> vias we need the drilled hole diameters and the plating
> thickness—the finished hole size is an anachronism left over
> from through-hole technology.
>
> Regards,
> Werner Engelmaier
> Engelmaier Associates, L.C.
> Electronic Packaging, Interconnection and Reliability Consulting
> 7 Jasmine Run
> Ormond Beach, FL 32174 USA
> Phone: 386-437-8747, Fax: 386-437-8737, Cell: 386-316-5904
> E-mail: [log in to unmask], Website: www.engelmaier.com
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV
> 1.8e To unsubscribe, send a message to [log in to unmask] with
> following text in the BODY (NOT the subject field): SIGNOFF
> Technet To temporarily halt or (re-start) delivery of Technet
> send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail
> to [log in to unmask]: SET Technet Digest Search the archives
> of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
|
|
|