Thanks, Tim - that'll teach me to go stirring pots with a touch of
facetiousness. Aluminiium, of course, is a case in point. It just struck me
as something of a contradiction that oxides should form on an alloy that
had earlier been described as uncorrodable. I'll go back to my corner now.
Peter
Tim Reeves <[log in to unmask]> 28/05/2003 01:28 AM
Sent by: TechNet <[log in to unmask]>
Please respond to "TechNet E-Mail Forum."; Please respond to Tim Reeves
To: [log in to unmask]
cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
Subject: Re: [TN] Sn-Ni PCB plating
Big mistaken assumption: uncorrodable = no oxide formation
Actually, the presence of a tough oxide film on the surface is what makes
certain metals corrosion resistant. Virtually all metals form oxides in the
presence of oxygen. It's the ability of that oxide film to "seal off the
surface" from further corrosion that's key.
Tim Reeves
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Sunday, May 25, 2003 9:15 PM
Subject: Re: Sn-Ni PCB plating
Happy,
As I read your post, plating Gold, tin, tin-lead, silver, Pd, etc would be
to provide a solderable surface, not to prevent oxides forming (since
tin-nickel is uncorrodable, there should be no oxides, right?). Gold is not
a finish that most people would want to solder to either as it causes
solder embrittlement. The others are OK. Gold is normally only used to
cover and protect another, solderable plated finish that DOES oxidise, but
it's so thin that it doesn't impact on solder joint quality. I've not come
across Gold as the material to actually solder to. Or have I missed a big
something?
Peter
Happy Holden <[log in to unmask]> 23/05/2003 10:40 PM
Sent by: TechNet <[log in to unmask]>
Please respond to "TechNet E-Mail Forum."; Please respond to HTH
To: [log in to unmask]
cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
Subject: Re: [TN] Sn-Ni PCB plating
Good question Jack,
The property that makes it uncorrodable (a very thick-non porous oxide
film) also makes it very difficult to solder. In the old days we could use
an active acid flux but that is no longer true. The current non-clean type
of flux would not even penetrate the oxide on a tin-nickel pad and it would
end up non-wetted (not even de-wetted). Gold, tin, tin-lead, silver, Pd,
etc all solder very nicely, so they need to be put over the tin-nickel to
prevent the oxides from forming.
The other factor is that the plating bath is difficult to control and you
have to watch it to make sure it does not plate stressed. I once saw the
traces 'jump' off the boards after etching, the tin-nickel was so stressed.
But like I said, the sail boat metal parts are remarkable!
Happy
"Jack C. Olson"
<[log in to unmask]> To: TechNet
<[log in to unmask]>
cc: [log in to unmask]
05/23/2003 09:32 AM
Subject: Re: Sn-Ni
PCB plating
Ok, I'm probably showing my ignorance here,
but with a stable non-corrodable finish like
Sn-Ni, why do you need the gold?
Jack (a PCB layout guy)
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|