TECHNET Archives

February 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Robert Coburn <[log in to unmask]>
Date:
Wed, 7 Feb 2007 09:00:47 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Marsico, James" <[log in to unmask]>
Subject:
From:
"Marsico, James" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (57 lines)
I haven't found an industry standard, but did find a company offering this service, Corfin Industries.  They call it Tin Whisker Mitigation.  
http://www.corfin.com


 Jim Marsico
EDO Corporation
1250 New Horizons Blvd.
North Amityville, NY 11701
631-630-5079
[log in to unmask]

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Coburn
Sent: Wednesday, February 07, 2007 8:45 AM
To: [log in to unmask]
Subject: [TN] Hot solder dip to mitigate Sn whiskers

Hi T'netters;
My emails can't get through using my work address so hopefully this 
alternate e-dress works.

My questions are:
Does anyone pre-treat pure tin finish terminations on components with a hot 
solder dip to mitigate tin whiskers?
Is there an industry standard on this process?

TIA;

Regards,
Rob Coburn
TDI
[log in to unmask]

_________________________________________________________________
Turn searches into helpful donations. Make your search count. 
http://click4thecause.live.com/search/charity/default.aspx?source=hmemtagline_donation&FORM=WLMTAG

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2