TECHNET Archives

November 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Dieselberg, Ron" <[log in to unmask]>
Date:
Mon, 22 Nov 1999 15:42:08 -0500
MIME-Version:
1.0
X-To:
"Ingemar Hernefjord (EMW)" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Dieselberg, Ron" <[log in to unmask]>
Parts/Attachments:
text/plain (55 lines)
Ingemar, you might try Chromerics. They made some conductive gaskets for us
some time back.
Chromerics Div.
77 Dragon Ct.
Woburn, Mass 01888-4014
781-935-4850

Ron Dieselberg

-----Original Message-----
From: Ingemar Hernefjord (EMW)
[mailto:[log in to unmask]]
Sent: Friday, November 19, 1999 02:24
To: [log in to unmask]
Subject: [TN] Ku-band waveguide gasket


Hi, an unusual question, but I see many radar guys are reading also in
TechNet. So, what sealing gaskets do you use for flange-to-flange sealing,
electrically as well as gas tightening? We tried Indium, works well, but the
price is immense. If the waveguide is ordinary Al with Nickel+Chromate, then
what about Tin gaskets? Atmosphere around is dry and you have that Nickel
barrier. Copper seems to be too hard. Any good idea?
Ingemar Hernefjord
Ericsson Microwave Systems

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2