Jason, If you are looking for an NDI method, we use an ultrasonic
instrument called a Positector 100-B3 ... it requires the use of a couplant
liquid, but has a small transducer footprint size. It is designed to
measure cured coating thicknesses on fiberglass or similar. It is made by
Defelsko Instruments (website: www.defelsko.com)
Sheila
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of McMonagle, Mike
Sent: Tuesday, February 22, 2000 3:28 PM
To: [log in to unmask]
Subject: Re: [TN] Conformal Coating Thickness Gauge
Jason,
The easiest way is to take a sample of the actual product (or bare
laminate if you can't sacrifice the product), subject it to the coating
process, then cross-section and measure (visually or mechanically) the
results against an uncoated sample.
Mike
-----Original Message-----
From: Jason Gregory [mailto:[log in to unmask]]
Sent: Tuesday, February 22, 2000 2:05 PM
To: [log in to unmask]
Subject: [TN] Conformal Coating Thickness Gauge
Hello everyone,
Can anyone direct me to the best way (or inspection equipment) to inspect
the thickness on conformal coatings? TIA.
Jason Gregory
Production Manager
Electrospec
(713)784-4900
(713)784-1194 fax
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|