TECHNET Archives

May 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Nancy Trumbull <[log in to unmask]>
Date:
Fri, 26 May 2000 07:39:22 -0400
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Nancy Trumbull <[log in to unmask]>
Parts/Attachments:
text/plain (53 lines)
Good morning David,
I don't know the answer to your question but I did post it on the trainer net.
Good luck and have a save and happy holiday.
Nancy T

>>> [log in to unmask] 05/25/00 04:56PM >>>
I was hoping to get some help from you IPC standards experts out there.

I was looking for the IPC standard that is violated when copper is exposed
on a gold finger card edge connector.  The copper that I am seeing is a
result of a chamfer that cuts an internal layer of the PCB.  The spec is for
.035 material removed along gold finger and .020 removed in the PCB's
thickness.  I expect analysis will prove that this spec is being violated.
I know that exposed copper is a violation but I cannot find a standard that
proves this in this scenario.

On a similar note, when ordinary gold fingers are made correctly and have a
chamfer, copper is exposed when the chamfer cuts into the gold finger
plating.  If this is a correct statement, why is this not a violation due to
corrosion of the exposed copper?

Thanks in advance

David Romero

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2