TECHNET Archives

May 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Engelmaier <[log in to unmask]>
Date:
Fri, 8 May 1998 00:51:12 EDT
Content-transfer-encoding:
7bit
Content-type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Engelmaier <[log in to unmask]>
Parts/Attachments:
text/plain (30 lines)
Jo,
Unfortunately, the advice given that larger volume solder joints are more
robust is bad advice. Solder joints are robust when good wetting has taken
place and not otherwise. A properly wetted solder joint has all the strength
it ever needs except for some extreme HALT or HASS tests which are
inappropriate in the first place for solder joints. Studies hav shown, that
smaller solder fillets for in particular caps lead to higher reliability,
primarily because of reduced component cracking. Yield will also increase
because of a lower tendency of tombstoning.

Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL  32174  USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2