TECHNET Archives

June 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Phil Bavaro <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Mon, 16 Jun 2014 16:15:05 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
Hi Paul,

That is a pretty standard large package, 1.27 mm pitch, 25 x 25 mm BGA.  I haven't soldered one in many years but used to assemble that kind often without issues.

What kind of soldering problems are you having?

If it is corners only, the .2 mm coplanarity might be a problem.

Phil




-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Taylor
Sent: Monday, June 16, 2014 8:53 AM
To: [log in to unmask]
Subject: [TN] Soldering Issues on Freescale PGA357

Hi

new to the forum, although in a previous life I used it quite a lot!

We use the Freescale MPC860DTCZQ50D4 in one of our designs, we've had a few issues with soldering at our sub-contractor which has got worse as we just don't seem to be able to lock down the root cause.
We have other BGA's on the boards (different pitches) which solder ok

The problem is always the outer pins in the corners , I've a lot of infor on the tests we have done, but I had seem a post about contamination of the balls on the Motorola package, which to be frank I hadn't considered

I've also seen some info about substrate changes which I'm wondering if it also was connected
________________________________
 This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2