TECHNET Archives

October 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Tempea, Ioan" <[log in to unmask]>
Date:
Sun, 28 Oct 2007 10:33:31 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Hfjord <[log in to unmask]>
Subject:
From:
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (120 lines)
Ioan,

Twofold is good, threefold even better:
Quality!
If the platings are bad, thickness or thinness is meaningless to debate.
It's a pity, but we have seen many examples on questionable plating. With
all knowledge that exists today,there should be no such issues.

 The tin plating is seldom real bad, but the nickel plating is sometimes of
a kind, that nothing helps: unsolderable. If Peer's advice isn't working,
take some pictures on the anomalous pins and let us have a look at them, you
may have a quality problem too.

My two microinches

Inge


-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Tempea, Ioan
Skickat: den 26 oktober 2007 17:11
Till: [log in to unmask]
Ämne: Re: [TN] Component pins plating thickness

Thanks Peer,

so it's not the plating 8-{

Have to play a little bit more with the reflow, forgotten to mention the
connector is SMT.

Regards,

Ioan

-----Original Message-----
From: P. Langeveld [mailto:[log in to unmask]]
Sent: Friday, October 26, 2007 10:48 AM
To: TechNet E-Mail Forum; Tempea, Ioan
Subject: Re: [TN] Component pins plating thickness


Ioan,

 The answer is 2-fold:

1. The measured finish layers are OK. The manufacturers spec however
are, too lean.  Already in the lead age the Ni-layer should be 0.002
mm (80 microin), the minimum Sn thickness 0.005 mm (200 microin).
Otherwise the risk of the Sn layer is not hermetic sealing the Ni
layer and the latter can be oxidized. And give wetting problems, and
even more in PTH's.

2. I presume the connector is wave soldered at say, 265 dC.
The (matte) tin has a melting point of 231 dC. Added with the thermal
mass of the internal metal contact lips and other internal heat sinks
in the board, the (total) contact time on the wave(s) has to be
increased with about 1 second.

Success.

Peer Langeveld
Consultant Soft Soldering Processes
5502 VH 8 The Netherlands

2007/10/26, Tempea, Ioan <[log in to unmask]>:
> Hi Technos,
>
> I'm having a tough connector here, hard time to get all the pins soldered.
>
> It is matte Sn over Ni finished, measured coating thicknesses are 250
microinch Sn over 80 microinch Ni. Are these values OK? Isn't the Ni too
thin and the Sn too thick?
>
> The manufacturer spec is 0.001mm (40 microin) minimum Sn over 0.0013 (51
microin) minimum Ni.
>
> Thanks for your input,
>
> Ioan
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2