>At 02:21 PM 11/14/96 PST, you wrote:
>Is there an electrically conductive adhesive which will survive a reflow 
>at 220-240 C while maintaining reasonable bond strength?  Probably not, 
>but I thought I'd ask anyway.
>
>
>[log in to unmask]
>
Steve,

Epoxy Technology Inc., Billerica MA, Tel. (508) 667-3805, (800) 227-2201
has a Conductive Epoxy, Type H20E, which is specified to have 16oz of shear
strength at .1"x.1 pad. It can be cured at 175 degrees C for 45 sec, or at
lower temperatures, but longer. 

Tra-Con, Bedford MA, Tel (800) TRA-CON1 has also a Conductive Epoxy, but I
have no specs. at hand.

I am not sure whether this is the type of 'adhesive' you meant. In any case
I hope it will help you.

Rolf Ehrat
Sen. Des. Eng.
Scintrex Ltd.
Concord, Ont.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2