TECHNET Archives

April 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
"Coleman, Bill" <[log in to unmask]>
Date:
Fri, 11 Apr 2003 17:10:15 -0600
MIME-Version:
1.0
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Morse, Carrie" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Coleman, Bill" <[log in to unmask]>
Parts/Attachments:
text/plain (111 lines)
Check IPC 7525.  There is a section in there about intrusive reflow.  Two
Print stencils are good for situations where there is not enough real estate
for overprint.  We have several customers using Two Print Stencils.

William E. Coleman
Vice President - Technology
Photo Stencil An ISO 9001 Registered Company
4725 Centennial Blvd.
Colorado Springs, CO 80919
Phone # 719-535-8528
Fax #      719-599-4334
Cell #      719-331-2433
email:      [log in to unmask] <mailto:[log in to unmask]>

        -----Original Message-----
        From:   Morse, Carrie [SMTP:[log in to unmask]]
        Sent:   Friday, April 11, 2003 9:37 AM
        To:     [log in to unmask]
        Subject:        Re: [TN] Apertures for intrusive reflow

        You might get bridging.  You might not.
        If there is sufficient surface tension to pull the solderpaste into
the hole, then, you
        probably won't get bridging.  If the surface tension is
insufficient, you may end up with a large solder ball between the pins.  I
think that scenario is more likely than the bridge considering the wide
pitch.  The only way to really know is to try it.  I'd also be concerned
about some solder joints getting more solder than others (one scavenging
from the other)

        -Carrie

        -----Original Message-----
        From: Tempea, Ioan [mailto:[log in to unmask]]
        Sent: Friday, April 11, 2003 8:22 AM
        To: [log in to unmask]
        Subject: [TN] Apertures for intrusive reflow


        Hi Technos,

        I am investigating intrusive reflow and big part of the topic is OK
for me.
        I learned how to calculate the volume of the paste, I even tried the
process
        on several assemblies, all OK.

        Now I'm running into a board with less real estate, so not so much
space to
        do the overprinting. According to my calculations the apertures for
this
        particular TH connector would overlap. It's a 78.7 mils pitch.

        The question is: could I overlap the apertures and print paste all
over,
        bridging between the pins? Since we deal with large pitch and we're
talking
        liquid paste flowing towards the holes, would this not create solder
bridges
        after reflow?

        Thanks for your insights,
        Ioan

        ---------------------------------------------------
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8e
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
        To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
        Search the archives of previous posts at:
http://listserv.ipc.org/archives
        Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
        -----------------------------------------------------

        ---------------------------------------------------
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8e
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
        To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
        Search the archives of previous posts at:
http://listserv.ipc.org/archives
        Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
        -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2