Paul,
"Threadlockers" is the name usually given the anaerobic adhesives. They
cure in the absence of oxygen and in the presence of metal ions.
Consequently, anaerobics are used for metal bonding, like bonding gears
to shafts. They would not be suitable for plastics, if that is the case
in your scenario.
Is the issue that you have two parts to mix? Perhaps a single part,
electronics grade RTV silicone could be considered.
Regards,
Peter
--------------------------------------------------------
Peter Swanson [log in to unmask]
INTERTRONICS http://www.intertronics.co.uk
Tel: +44 1865 842842 Oxfordshire, England
INTERTRONICS is dedicated to providing quality material, consumable
and equipment solutions to the high technology, high performance
assembly industries, incorporating outstanding levels of technical
support and customer service.
Read our news! http://www.intertronics.co.uk/blog/blog.htm
INTERTRONICS is the trading name of Cygnet Electronics Ltd,
registered in England No 1835617. Registered office:
17 Station Field Industrial Estate, KIDLINGTON, Oxfordshire, OX5 1JD,
ENGLAND.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul O Connor
Sent: 10 September 2010 11:59
To: [log in to unmask]
Subject: [TN] IP67 - Gland + Threadlocker
Hi,
My company has a product that is IP67 rated (Waterproof) there are cable
glands that are fitted (threaded) to a polycarbonate case - I use a 2
part epoxy to seal thse glands at present does anyone know of a type of
threadlocker gel that would give the same result?
Thanks
Paul
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|