TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0ukvrm-0000OaC; Mon, 29 Jul 96 12:12 CDT
Content-Type:
TEXT/PLAIN; CHARSET=US-ASCII
Old-Return-Path:
Date:
Mon, 29 Jul 1996 10:19:52 -0700
Precedence:
list
Reply-To:
cc:
MIME-Version:
1.0
Status:
O
Priority:
Normal
TO:
Return-Path:
<TechNet-request>
X-Status:
From [log in to unmask] Tue Jul 30 12:
04:19 1996
X-Loop:
Resent-Message-ID:
<"qz8iy3.0.yBC.u3F_n"@ipc>
Subject:
From:
Michael Barmuta <[log in to unmask]>
X-Mailing-List:
<[log in to unmask]> archive/latest/5420
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
Message-Id:
Parts/Attachments:
TEXT/PLAIN (76 lines)
	To cmaffe:							
									
		In the past we carbon treated our acid copper plating baths 
on a time basis as you are curently doing.About 10 years ago we switched from 
a time accumulation basis to an amperage basis.We are currently carbon 
treating when 600 Amp Hours/Gal.is reached.				
		The following factors were used to arrive at this number:	
		1.Plating distribution, surface:hole			
		2.Surface plating distribution,top of the top racked 	
		panel:bottom of the bottom racked panel			
		3.Cross sections;  grain structure and corner cracking	
		4.Ductility                                                  
    		5.Hull cell						
									
		These are Lea Ronal PCM+ baths with automatic brightner 
dosig.All plating is pattern plate with Dynachem LP resist.The carbon treat 
cycle uses an oxidizer followed by the carbon all done off line in a batch 
process.This should provide you with a starting point.Obviously many factors 
can influence your requirement;resist,chemisties-preclean/acid 
copper,rinsing,carbon treat procedure,end user specifications etc.etc.	
									
					Regards				
					Michael Barmuta			
					Staff Engineer			
					Fluke Corp.			
					Everett Wa.			
					(206)356-6076			
								 	
		
On Mon, 29 Jul 1996 07:06:29 -0700 [log in to unmask] wrote:

> From: [log in to unmask]> Date: Mon, 29 Jul 1996 07:06:29 -0700
> Subject: Carbon Treatment
> To: [log in to unmask]
> Cc: [log in to unmask], [log in to unmask], [log in to unmask]
> 
>      With higher tech product these days and the associated high aspect 
>      ratio copper plating chemistries, we're looking for a good method to 
>      determine when to carbon treat as a preventative measure.  For years 
>      I've used a guideline of carbon treating copper baths every 6 mos. or, 
>      if through put per gal was very high, perhaps quarterly.
>      
>      T&E results are so susceptible to sample prep, and I've never really 
>      found them to correlate to anything but perhaps extreme organic 
>      contamination.  I've never felt comfortable relying on those to 
>      indicate when to treat. 
>      
>      Multiple thermal shock is another method I'm hearing is an indicator. 
 
>      We currently pass six or more, yet just went through a bath decant to 
>      minimize detrimental organic build up while awaiting installation of a 
>      new carbon treatment system.  The baths are only about 6 mos. old but 
>      with only about 3 months of production throughput.
>      
>      Appreciate any ideas or schemes that work for others, especially high 
>      volume, high tech.
> 
> ***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 *
> ***************************************************************************
> * To unsubscribe from this list at any time, send a message to:           *
> * [log in to unmask] with <subject: unsubscribe> and no text.        *
> ***************************************************************************
> 



***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2