TECHNET Archives

December 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Alan Kreplick <[log in to unmask]>
Date:
Wed, 3 Dec 1997 10:34:59 -0500
Content-type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Alan Kreplick <[log in to unmask]>
Parts/Attachments:
text/plain (27 lines)
A few questions on bar solder used in the wave solder process . . .


Are all bar solders alike?  All claim to exceed the requirements of
J-Std-006.

Are there any substantial differences between ultra-pure, virgin, etc.?

Any advantage/disadvantage between 60/40 & 63/37?

Is there in easy method to evaluate the solder performance other than
dumping 1000+ pounds of solder and re-filling with the new solder?

Or does it just come down to cost (per pound)?

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2