Pat,
I have never attempted to use anodized aluminum wire before, but have
frequently used PURE 1.25 - 20 mil diameter aluminum wire for wire bonding
in automotive and power applications.
You can try the following three sites. I KNOW they can provide the wire
diameter you want, but it may be too pure for your needs. Normal wire
bonding wire is very pure, and hence, very soft.
What I DO NOT know, is if they will anodize it for you. I rather doubt it,
but then it is worth a phone call.
May I be inquisitive and ask why one would use anodized aluminum wire of
this diameter??
http://www.semx.com/companies/spm.asp - SPM
http://www.williams-adv.com/ - Williams
http://www.kulickeandsoffa.com/ - American Fine Wire
Best of luck,
Steven Creswick - Gentex Corp
-----Original Message-----
From: Diamond, Pat [mailto:[log in to unmask]]
Sent: Friday, January 11, 2002 3:29 AM
To: [log in to unmask]
Subject: [TN] Anodised Aluminium wire
I am looking for information on a supplier for anodised aluminium wire, the
problem is that the wire must be between 005" and 006" in diameter.
Can anyone help?
regards,
Pat Diamond
Weston Aerospace
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To recieve ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To recieve ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|