hi,
from time-to-time you may encounter components that may use a low temperature solder in their construction (integrated microwave assemblies for example). in these cases, batch reflow of high temperature solder will surely reflow the low temperature solder inside these packages. as you know, fudge answers can get you into deep doo-doo.
phil
-----Original Message-----
From: <Peter George Duncan> [mailto:[log in to unmask]]
Sent: Wednesday, May 23, 2001 2:58 AM
To: [log in to unmask]
Subject: [TN] Component Failure Temperatures
Morning, All,
I need a quick and general answer to the question "What typically is the
temperture at which components come apart/melt?" My boss asked me how the
use of high melting point (221 deg C) solder would affect components in the
CR Oven, and all I could give him was a fudge answer about thermal profiles
and how even MIL spec devices (rated at 125 deg C) survive 215 deg C+
during soldering with 63/37 solder. Does anyone have an idea of the rough
temperature at which Industrial grade (-40 to +85 deg C) platic-bodied
components fry, and how long it takes to fry them at that temperature?
I had a look through randomly selected component data sheets, but none of
them contained this useful bit of information. They state that if the
maximum case temperature is sustained for an unspecified time, it could
affect the performance and/or reliability of the device, but they advice
was totally non-specific about exactly how much for how long. I experienced
using a component once that had to be manually soldered because it kept
falling apart internally whenever it went near a soldering machine, so I'm
cautious about giving uninformed replies.
I'm trying to solder 35 x 35 mm PBGA's (318 and 388 pins) to an FR4 board
with a finish of 4.5 microinches gold over 150 microinches of Nickel. HMP
solder has been recommended, but the temperature that the boards are
exposed to during soldering goes up by 35 deg C over normal. Your advice,
stories, etc. much appreciated.
Pete Duncan
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|