REFER TO IPC 6012 SECTIONS 3.10.2 & 3.10.2.1 also MAY LOOK AT Table 4-3

----------
> From: Paul Robertson <[log in to unmask]>
> To: [log in to unmask]
> Subject: [TN] Bare Board Cleanliness
> Date: Friday, November 07, 1997 7:04 AM
>
> Could anyone provide me with the IPC standard relating to incoming bare
PCB
> cleanliness.
> Any information would be appreciated
>
> Regards
> Paul Robertson
> Paul Robertson
> Engineering Section Leader
> PCB Assembly
> Schlumberger Electricity
> Langer Road, Felixstowe, Suffolk, IP11 8ER, UK
> Phone    : +44 (0) 01394-694-417  (Direct)
> Fax      : +44 (0) 01394-694-319
> Email    : [log in to unmask]
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2