TECHNET Archives

August 2017

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 29 Aug 2017 16:31:07 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Yuan-chia Joyce Koo <[log in to unmask]>
Message-ID:
Subject:
From:
Yuan-chia Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"; delsp=yes; format=flowed
MIME-Version:
1.0 (Apple Message framework v753.1)
Parts/Attachments:
text/plain (50 lines)
adhesion not adhesive... correction...
On Aug 29, 2017, at 4:29 PM, Yuan-chia Joyce Koo wrote:

> aluminum wire bond?  usually no problem on quartz, unless you  
> directly bond  on top of the structure (MEMS for example).  As for  
> gold plating lift off, either you have over travel of bond head  
> (wedge), smash (force) too much, or your gold seed layer adhesive  
> not strong enough (chemical seeding, instead of good   
> sputtering)... IMHO (old info... more than 10 year old.. for your  
> reference only).
> jk
> On Aug 29, 2017, at 1:49 PM, Ioan Tempea wrote:
>
>> Dear Technos,
>>
>> Does any of you have experience with wire bonding on quartz  
>> components?
>>
>> Can ultrasonic bonding damage quartz or can it lift the Au plating  
>> from the quartz base material?
>>
>> Any process related suggestions?
>>
>> Thank you,
>>
>> Ioan Tempea, P. Eng.
>> Senior Manufacturing Engineer, Satellite Systems
>>
>> [cid:[log in to unmask]]
>>
>> MacDonald, Dettwiler and Associates Corporation, 21025 Trans- 
>> Canada Highway, Ste-Anne-de-Bellevue, QC, Canada H9X 3R2
>> Tel: +1-514-457-2150 x3556
>> www.mdacorporation.com<http://www.mdacorporation.com/>
>>
>> This e-mail, and any attachments, are intended solely for the use  
>> of the intended recipient(s) and may contain legally privileged,  
>> proprietary and/or confidential information. Any use, disclosure,  
>> dissemination, distribution or copying of this e-mail and any  
>> attachments for any purposes that have not been specifically  
>> authorized by the sender is strictly prohibited. If you are not  
>> the intended recipient, please immediately notify the sender by  
>> reply e-mail and permanently delete all copies and attachments.  
>> This email is for informational purposes only and shall not be  
>> interpreted to authorize or conclude a binding agreement between  
>> MDA and any other party unless this email contains or is  
>> accompanied by an express written confirmation of MDA's intention  
>> to enter into a binding agreement, such confirmation shall only be  
>> provided by an authorized representative of MDA.

ATOM RSS1 RSS2