TECHNET Archives

August 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Graham Naisbitt <[log in to unmask]>
Date:
Fri, 9 Aug 2002 12:20:47 -0400
Reply-To:
Subject:
From:
Content-Transfer-Encoding:
7bit
In-Reply-To:
<001d01c23faf$de034c60$f841c0c1@vaio>
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (185 lines)
Graham
how long you immerse the PWB in "hot" IPA/DI mixture?  what is "hot"?
jk

>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]]On Behalf Of Graham Naisbitt
>Sent: Friday, August 09, 2002 10:20 AM
>To: [log in to unmask]
>Subject: Re: [TN] Board cleanliness
>
>
>Hi Bev and Susan,
>
>Permit me a  W O A H!
>
>This is such a misleading spec. To say that something should be cleaned
>to a level of less than 1.5 microgrammes / cm2 also means that it is
>acceptable to leave UP TO 1.5 microgrammes of NaCl equivalence on every
>square cm of your assembly! But if you are manufacturing to modern
>fine-line, fine-pitch and components to suite....then that level will
>almost certainly be too high.
>
>I have many customers who have, as a result, imposed their own empirical
>cleanliness value at something less than 0.02microgrammes/cm2 for Class
>3 assemblies. As has been stated already, the ionic extract cleanliness
>test is/was only intended to be used for process monitoring. The
>Pass/Fail can and has got a lot of people into troublesome problems.
>
>I also register concern at the use of "hot" ipa / water mixture - safety
>issues apart, there has been a good deal of research demonstrating that
>prolonged immersion in such a solution can induce the bromine flame
>retarder to rise to the surface of the board and....this is a problem!
>Would you care to comment?
>
>Regards Graham Naisbitt
>
>[log in to unmask] <mailto:[log in to unmask]>
>
>Concoat ANNOUNCE their acquisition of the former Multicore SPCID
>business.
>
>MUST II Solderability Testing Systems -
>CM Cleanliness Testing Systems -
>Auto-SIR Reliability Testing Systems -
>SoldaPro & NEW SoldaPro Wizard Thermal Profilers
>
>For more information please visit our new web site:
>www.concoatsystems.com <http://www.concoatsystems.com>
>
>Concoat Limited
>Alasan House, Albany Park
>Camberley GU16 7PH - UK
>
>www.concoat.co.uk <http://www.concoat.co.uk>
>
>Phone: +44 1276 691100
>Fax: +44 1276 691227
>Mobile: +44 79 6858 2121
>
>
>> -----Original Message-----
>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
>> Sent: Friday, August 09, 2002 03:44
>> To: [log in to unmask]
>> Subject: Re: [TN] Board cleanliness
>>
>>
>> Patrick,
>> Susan mentions a standard (US military MIL-P-55110E), but I
>> would like to point out another standard - GR-78 CORE from
>> Telcordia, which is used extensively in the
>> telecommunications industry.  It requires that the finished
>> bare board cleanliness be less than (or equal to?) 1
>> ug/square centimeter.  For you Americans, that's 6.5
>> ug/square inch.  The standard goes on to state that for a
>> finished assembly that has gone through a wash cycle that the
>> circuit pack have a SEC value less than (or equal to?) 1.5
>> ug/square centimeter.  There is no standard for no-clean
>> boards, but then there are other criteria that the no-clean
>> flux/solder paste must meet first
>> - copper mirror, halide ion spot test, SIR and
>> electromigration. Some companies still require a fluoride ion
>> spot test and SIR/EM testing of possible mixtures of wave
>> soldering fluxes/solder pastes/cored wires. And some
>> companies have set process indicator levels for SEC testing
>> of circuit packs manufactured with no-clean fluxes,
>> especially for wave soldering. Note, I said "process
>> indicator", so don't bring fire and brimstone down on me,
>> fellow Technetters!  :)
>>
>> regards,
>> Bev Christian
>> Research in Motion
>>
>> -----Original Message-----
>> From: [log in to unmask] [mailto:[log in to unmask]]
>> Sent: August 8, 2002 4:41 PM
>> To: [log in to unmask]
>> Subject: [TN] Board cleanliness
>>
>>
>> Hi Technetters,
>>
>> I would like to know how to specify board cleanliness on the
>> Fab drawing. We use class 3  boards. Does it make any
>> difference on cleanliness standard? Is it OK to ask for
>> cleanliness test results/reports shipped with every lot?
>> Which department in a company should be responsible for this
>> board cleanliness issue, R&D, Quality or Production?
>>
>> Thanks in advance to everyone sharing this information.
>>
>> Best regards,
>>
>> Patrick
>> ----------------------------------------------------------
>> This e-mail may contain SEL confidential information.  The
>> opinions expressed are not necessarily those of SEL.  Any
>> unauthorized disclosure, distribution or other use is
>> prohibited.  If you received this e-mail in error, please
>> notify the sender, permanently delete it, and destroy any
>> printout.  Thank you.
>>
>> --------------------------------------------------------------
>> --------------
>> -----
>> Technet Mail List provided as a free service by IPC using
>> LISTSERV 1.8e To unsubscribe, send a message to
>> [log in to unmask] with following text in the BODY (NOT the
>> subject field): SIGNOFF Technet To temporarily halt or
>> (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
>> http://listserv.ipc.org/archives Please visit IPC web site
>http://www.ipc.org/html/forum.htm for additional information, or contact
>Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
>------------------------------------------------------------------------
>----
>-----
>
>------------------------------------------------------------------------
>---------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text
>in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
>or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
>Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
>posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
>archives of previous posts at: http://listserv.ipc.org/archives Please
>visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>ext.5315
>------------------------------------------------------------------------
>---------
>
>-------------------------------------------------------------------
>--------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail
>to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>-------------------------------------------------------------------
>--------------
>

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2