electroless nickel plating on aluminum using a double zincate process
is available from ATOTech USA, Inc. It is a standard process and has
been in use for quite some time in various other industries.
Try calling Larry Loerch, 908.302.3529
Michael Holan
Process Engineer
HADCO-Austin
512-246-5600
______________________________ Reply Separator _________________________________
Subject: [TN] AW: [TN] Electroless Nickel for Aluminum
Author: =?iso-8859-1?Q?N=FCchter_Wolfgang_=28FV/FLT=29_=2A?=
<[log in to unmask]> at SMTPLink-Hadco
Date: 11/17/98 4:07 PM
Hi Mike,
As far as I know, you have to do a zincate treatment to get a good adhesion
between Al and Ni.
This process is not yet really a standard process available on the market,
but will be in the near future.
My purpose is to have an an wetable surface for solder in the case of
flip-chip. So try to contact Flip-Chip Technologies, IZM Berlin, Germany,
IBM, Motorola, IC Interconnect, ...
Hope this points you to the right direction.
Regards
Wolfgang Nuechter
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|