TECHNET Archives

July 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Rex Waygood <[log in to unmask]>
Date:
Wed, 2 Jul 2008 11:23:44 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bob Willis <[log in to unmask]>
Subject:
From:
Bob Willis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (129 lines)
For those not familiar smart-e-link forum is similar to the IPC groups and
using the same software so you can search the archives for the forum at 
http://lists.smartgroup.org/scripts/wa-SMARTGROUP.exe?A0=SMART-E-LINK 

Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
 
www.ASKbobwillis.com
 
New Bob Willis "Printed Board Inspection & Quality Control Workshop" 3rd
September www.ASKbobwillis.com/PCBworkshop.pdf 
 
Book your place on Bob's "Step by Step Failure Analysis Workshop" 11th
September  www.ASKbobwillis.com/faworkshops.pdf
 
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Rex Waygood
Sent: 02 July 2008 10:39
To: [log in to unmask]
Subject: Re: [TN] Silver-Palladium termination SMT solder problems

There has been a similar thread on smart-e-link in the last week.
The general consensus was that AgPd terminations are not compatible with
SAC.
Rex


Rex Waygood
Technical Manager
 
PartnerTech Poole Ltd 
Benson Road
Poole
Dorset BH17 0RY
United Kingdom
 
Tel: +44 (0)1202 674333
Fax: +44 (0)1202 678028
DDI: +44 (0)1202 338222
Mob: +44 (0)7887 997403
 
[log in to unmask]
www.PartnerTech.co.uk

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Grant Emandien
Sent: 02 July 2008 10:20
To: [log in to unmask]
Subject: [TN] Silver-Palladium termination SMT solder problems

Hi all,
 
We are experiencing poor solderability with AgPd-terminations on MOVs
exposed to a lead-free reflow profile using a SAC alloy on an
ENIG-finished PCB. Though we have run this board only once previously
with the same part finish using a lead-rich alloy, we had similar
effects but not to the extent we are now experiencing.
 
Can anyone provide some insight into this/
 
Regards
Grant
 

**********************************************************************
Relevant company disclaimers are available at the following addresses:
  Tellumat (Pty) Ltd e-mail:
mailto:[log in to unmask]
  Web:   http://www.tellumat.com/email.aspx
**********************************************************************

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


----------------------------------------------------------------------------
---

The information contained within this e-mail and any attachments contained
therein may be confidential and/or legally privileged and is for the use of
the intended recipient only. If you are not the intended recipient please
delete it from your system and notify the sender by return e-mail. The
content of this e-mail may not be copied or disclosed to any third parties
without prior permission from the sender. 

 

E-mail is susceptible to data corruption, interception, tampering and
viruses. We do not accept any liability for any such incidents or any
consequences thereof.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2