We have been using "no-clean" for some time now. Yes, when exposed to alcohol,
a white residue does result. I believe that this residue is benign, although
rather unsightly.
By customer request we have been asked to remove no-clean residue for
particular cards (due to customer concerns of effects the residue may have on
conformal coating). In that instance we cleaned the cards in our in-line
aqueous wash system using a suitable saponifier. We use an Alpha saponifier. I
imagine other flux suppliers make saponifiers as well.
Regards Evan
Evan Jones
Manufacturing Engineer
Bluegum Technology
Ph 61 3 5720 2539 Fax 61 3 5720 2412
Email [log in to unmask]
---------------------- Forwarded by Evan Jones/Australia/IBM on 13/02/98 15:21
---------------------------
[log in to unmask] on 13/02/98 01:53:16
Please respond to [log in to unmask] @ internet
To: [log in to unmask] @ internet
cc:
Subject: [TN] What can I use to clean my boards after rework if I am
Hi everybody I am having a problem, and it is that we used to use Water
soluble paste in the past and for that we used Alcohol to clean reworked
boards. Now we are in No-Clean and if we use alcohol there are some white
residues that sometimes bothers me a lot. Could somebody tell me more about
this white residues, how can I clean them, what can I use, are they
acceptable. This is urgent to me I will appreciate all your help.
Gracias,
Rub?n E. Irizarry-Guzm?n
Operations Engineer
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|