TECHNET Archives

February 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Date:
Sun, 11 Feb 2001 14:40:36 +0800
Content-Type:
text/plain; charset="us-ascii"
X-cc:
Gilbert Min <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, PCBA <[log in to unmask]>
Parts/Attachments:
text/plain (27 lines)
>"What is the Rolling Press?"
>Thanks
>Best regards / Gilbert Min

...it's a continues press for making FR4 laminates. Glassfabric and
copperfoil is continuesly feed to the press and you can make in theory
laminate sheets as long as the fabric or foil lasts. Dielektra Germany (now
ParkNelco) uses one for their thincores.

Because of heat transfer issues it's mainly used for thincore material and
will probably not work well on 1.60mm material. It can only be used to make
double sided laminates.

I think that is what it is.

Jens Behrens

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2