TECHNET Archives

March 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Date:
Mon, 1 Mar 2010 10:39:45 +0000
Reply-To:
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (124 lines)
Yes tin alloys tend to be yellow hue. However the hue you get on solders is
slight and is more easily determined by eye in side by side comparison to
another solder alloy. E.g. Lead alloys are slightly blue grey, silver
containing alloys are "warm" looking and so on, but I wouldn't use oxide
colour as a firm diagnostic. This is because 
- these colour differences only seem to be visible to people who are around
metals a lot.
- you can get interference effects with thin oxide films (similar to oil on
water) so colour can vary considerably from the normal typical slightly
yellow appearance of high tin alloy.

Regards
 
Mike

 -----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of R Sedlak
Sent: Saturday, February 27, 2010 8:26 AM
To: [log in to unmask]
Subject: Re: [TN] Colour of Oxidized Tin

Paul:  Your question is not really answerable, however you spell it!  The
term "oxidized" is usually thought to mean "reacted with Oxygen", but in the
strict chemical sense, (and in the real world) it can mean reacted with
anything, where the metal no longer has the full count of electrons.  And
what it has reacted with will profoundly affect the colo(u)r.
This is further complicated by the fact that Tin has two oxidation states,
+2 & +4...
You can't tell if it is Tin by the colo(u)r!
Rudy Sedlak
RD Chemical Company 

--- On Fri, 2/26/10, Paul Reid <[log in to unmask]> wrote:

From: Paul Reid <[log in to unmask]>
Subject: [TN] Colour of Oxidized Tin
To: [log in to unmask]
Date: Friday, February 26, 2010, 1:28 PM

Hi Everyone,

If we have oxidized tin what colour would you expect tin oxidation to
be.

I thought silver would oxidize black while tin might be more yellow or
gold.

Notice I used the word colour because I am in Canada.


Sincerely, 
Paul Reid 

Program Coordinator 
PWB Interconnect Solutions Inc. 
235 Stafford Rd., West, Unit 103 
Nepean, Ontario 
Canada, K2H 9C1 
613 596 4244 ext. 229 
Skype paul_reid_pwb 
[log in to unmask] <mailto:[log in to unmask]> 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------



      

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited.


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2