You know, something else was brought up on this forum not long ago. I almost forgot what I should
have remembered concerning delta Tg.

I know it's a long shot, but you might determine how well your supplier, and its supplier, effects
cure - especially with different materials or those MLB constructions with juicey or not so juicey
resin contents.

You can look back to December, I think, and see most folks don't allow in excess of 4 degrees C.
variance in Tg.

Again it's a long shot, but you might check if either DSC or TMA testing has been done to see.

Earl Moon

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2