TECHNET Archives

December 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
JH /Jørgen Hansen <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 1 Dec 1999 11:08:48 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (67 lines)
There will not be any reliability problems in Your case since the lenght of
the pressfit connection of the pin is shorter than full lenght of the pin,

>       Venlig hilsen
>      PRINTCA AS
>   Jørgen Hansen
> Production Technician
> *  +45 99 30 92 33      *  [log in to unmask]
> - - - - - - - - - - - - - - - - - - - - - - - - - - - - - - - - - -
> Printca AS
> Svendborgvej 3 - DK-9220 Aalborg Øst - Denmark
> Tel. +45 99 30 92 00   Fax +45 99 30 92 97
> http://www.printca.dk
> 


-----Oprindelig meddelelse-----
Fra: Lockley Neil [mailto:[log in to unmask]]
Sendt: 1. december 1999 10:29
Til: [log in to unmask]
Emne: [TN] Pressfit Connector Problem
Prioritet: Høj


Hi All,

I have a query with a Pressfit connector and a backplane. The only suitable
connector available has pins of 4mm in length and the backplane is 4.2mm
thick. Obviously the pins do not protrude through the PCB, will this cause
any problems with reliability, strength etc?

All comments appreciated

Cheers

Neil Lockley
Production Engineer,   TMSL.

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2