We use two methods.
1) peelable solder mask Techspray Wondermask P
2) holes with no plating through and about a 10 mil ring of no copper on the
inside diameter of the land.
-----Original Message-----
From: Ken Fong [mailto:[log in to unmask]]
Sent: Wednesday, January 17, 2001 12:48 AM
To: [log in to unmask]
Subject: [TN] Special through hole pad design
Technetters,
Could anyone advise a design of soldering pad which will not be closed with
solder during wavesoldering when the hole is not inserted with component,
but it
can form a normal solder joint when a component is inserted through the hole
with the lead clinched by auto-insertion machine? The board is 1.6mm thick
single sided pcb. Thanks.
Ken
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|